Skip to main content
Follow Us:
TOPCon Copper Plating Takes Another Step Forward: LIF

Editorial responsibility for this article rests with Wuhan Ooi Photoelectric Technology Co., Ltd. Written and reviewed by the Ooitech editorial team. See our editorial policy for how we write, where AI tools are used, and how to request a correction.

TOPCon Copper Plating Takes Another Step Forward: LIF

Quick answer: TOPCon copper plating moved a step closer to production with a new result building on earlier work from Jiangnan University. Plating replaces silver metallisation with copper, and the obstacle has never been the concept — it is adhesion and the barrier layer that keeps copper from diffusing into silicon. The process window in this study runs around 750 °C to 800 °C for the contact formation step, with a 1064 nm laser used in the patterning stage and annealing at 400 °C. Copper is roughly two orders of magnitude cheaper than the silver paste it would replace, and silver is the single largest non-silicon cost in a TOPCon cell. The remaining questions are line compatibility and long-term reliability: a plated contact that passes initial efficiency but degrades under damp heat is not a manufacturable process.

PV Module Manufacturing · by Jerry, Ooitech

Introduction

From the previous study to a new breakthrough

Yesterday we discussed a paper from Jiangnan University on TOPCon copper plating: laser grooving damages silicon, the crystallinity drops by 30 percentage points, and annealing is required to repair it. That paper concluded that 750°C annealing + HF cleaning could restore the efficiency from 23.41% back to 24.85%.

But anyone on a production line knows that 750°C annealing itself carries a hydrogen-induced blister risk — the temperature window is extremely narrow. Above 775°C the rear passivation layer blisters, and at 800°C the result is even worse than no annealing at all.

Is there a better way?

A second paper just published in 2026 by Jiangnan University + Jiangsu Xianghuan + DR Laser offers a new answer: use LIF (Laser-Induced Firing) to replace traditional low-temperature sintering, while simultaneously repairing the laser damage.

The results: efficiency improvement of +0.45% abs., Voc gain of 0.86mV, and — a major improvement in contact resistance uniformity.

1. A quick recap: the TOPCon copper plating flow and its pain points

The standard process and where it hurts

The standard TOPCon Ni/Cu plating flow:

Laser grooving → High-temperature annealing for damage repair → HF cleaning → Ni plating → Low-temperature sintering → Cu plating

Two pain points:

  • Laser grooving damages silicon: as discussed in the previous article, crystallinity drops from 99.3% to 69.8%, requiring high-temperature annealing for repair.

  • Traditional low-temperature sintering is non-uniform: the furnace heats the entire cell, edges dissipate heat faster while the center stays hotter, causing contact resistance to be high at the edges and low at the center — non-uniform current collection hurts FF.

The core breakthrough of this new paper: inserting LIF into the plating flow kills two birds with one stone — it replaces the non-uniform low-temperature sintering and assists in repairing the laser damage.

TOPCon Copper Plating Takes Another Step Forward: LIF Replaces Sintering, Efficiency +0.45% abs., Voc Damage Repaired

2. What is LIF, and how is it different from traditional sintering?

Furnace heating vs. point-to-point welding

Traditional low-temperature sintering: place the whole cell in a furnace and bake at 200–400°C. The problem is uneven heating — edges cool faster, the center gets hotter, and contact resistance varies significantly across the cell.

LIF (Laser-Induced Firing): a 1064nm infrared laser rapidly scans the front of the cell while a reverse bias (2–18V) is applied. The laser excites photogenerated carriers, the reverse bias drives them directionally, producing precise localized Joule heating at the metal–silicon interface.

TOPCon Copper Plating Takes Another Step Forward: LIF Replaces Sintering, Efficiency +0.45% abs., Voc Damage Repaired

One-sentence difference: traditional sintering is "whole-cell baking", LIF is "point-to-point welding". LIF only heats the contact region under the gridlines, leaving everything else thermally untouched.

Fig. 2

3. How well does LIF work on copper-plated cells?

Finding the sweet spot at 14V

Fig. 4

The paper first runs a baseline experiment: apply LIF at different reverse bias voltages on cells that have already completed Ni/Cu plating.

LIF Reverse VoltageEfficiencyVocFFRs
No LIF (baseline)24.29%696.27mV81.74%1.51mΩ
8Vimproving———
14V24.69%+0.32mV+1.22%1.16mΩ
16–18Vdropsdropsdrops sharplybasically unchanged

Optimal parameters: 14V reverse bias, efficiency gain +0.401% abs., FF gain 1.22%, Rs reduction 23%.

Why does higher voltage make things worse?

Fig. 5

The paper uses Suns-Voc to measure the dark saturation current densities J01 and J02:

  • J01 (representing pn-junction recombination): little change with voltage

  • J02 (representing metal–silicon interface recombination): lowest at 14V, soars at 16–18V

Translation: too much voltage means excessive Joule heating, and the interface gets "welded to death". The window sits right around 14V.

4. Why can LIF repair laser damage?

Raman spectroscopy reveals the secret

Fig. 7

The paper ran a key experiment: strip the plated metal off and use Raman spectroscopy to measure the crystallinity of the silicon under the gridlines.

ConditionCrystallinity
No LIF (only high-T annealing repair)~95%
LIF 8–14V+0.76% ~ 1.84%
LIF 16–18Vdecreases

On top of high-temperature annealing, LIF further pushes crystallinity higher.

The mechanism: LIF generates a localized instantaneous high temperature (far above traditional annealing temperatures) that allows amorphous silicon to recrystallize more completely, and it only heats the regions under the gridlines, leaving the rear passivation layer untouched.

Fig. 6

This solves the lingering concern from the previous article — the temperature window for high-T annealing is narrow, and above 775°C the rear passivation blisters. LIF is local heating; the rear is unaffected, so the temperature can go higher and the repair effect is better.

5. When should LIF be applied? Timing matters

Three candidates and a clear winner

The plating process has three steps: Ni plating → low-temperature sintering → Cu plating. Where should LIF be inserted?

Fig. 8

The paper compares three timings:

GroupLIF TimingOptimal VoltageBest EfficiencyCrystallinity
AAfter Ni, before sintering8V24.689%~95.6%
BAfter sintering, before Cu8V24.663%~96.45%
CAfter Cu14V24.69%Highest

Conclusion: LIF works best when placed at the very end — after Cu plating is complete.

Fig. 13

Why?

After Cu plating, electrode resistance drops dramatically. When LIF applies voltage, current distribution is more uniform, Joule heating is more uniform, and interface contact is optimized more thoroughly.

If LIF is applied only on the Ni layer (before Cu plating), the resistance is high; the same voltage produces excessive Joule heating, which can easily "weld the interface to death".

6. A bigger discovery: LIF can fully replace low-temperature sintering

Skipping the furnace altogether

If LIF can optimize the Ni–Si contact, then can we simply skip the traditional low-temperature sintering step entirely?

Fig. 9

The paper designed an experiment (Group D): Ni plating → LIF (8V) → direct Cu plating, skipping the low-temperature sintering step.

Results:

GroupProcessEfficiencyContact Resistance Uniformity (edge–center difference)
OTraditional sintering, no LIFbaseline3.53Ω
ANi+LIF+Sintering+Cu24.689%2.05Ω
BNi+Sintering+LIF+Cu24.663%1.46Ω
CNi+Sintering+Cu+LIF24.69%1.54Ω
DNi+LIF+Cu (no sintering)24.74%0.45Ω

Group D's contact resistance uniformity crushes every group that includes traditional sintering.

Fig. 11

Why?

Traditional sintering furnaces heat unevenly — edges dissipate heat fast, the center is hotter — causing contact resistance to be higher at the edges and lower at the center. LIF is a point scan; every point receives exactly the same energy, uniform by nature.

Further optimizing the LIF voltage to 6V, Group D reaches an efficiency of 24.74%, with Voc reaching 696.72mV — +0.45% abs. higher in efficiency and +0.86mV higher in Voc than the traditional sintering + no LIF baseline.

7. Production-line implications: is the mass-production threshold for copper plating lowered?

Three concrete advances

This paper delivers several tangible advances:

1. Voc damage can be repaired, and repaired better. The 750°C annealing from the previous article had a narrow temperature window and a risk of rear-side blistering. LIF heats locally, the rear stays safe, and the repair is more effective.

2. One process step is saved, but equipment investment must be weighed. Traditional flow: Ni plating → low-T sintering → Cu plating. LIF approach: Ni plating → LIF → Cu plating. Saves the sintering furnace and process time, but LIF equipment itself is more expensive, and integration with the plating line is more complex. The actual ROI depends on equipment quotations.

3. Contact resistance uniformity is the hidden bonus. Traditional sintering shows an edge-to-center contact resistance gap of 3.53Ω; the LIF approach cuts it down to 0.45Ω. Better uniformity means more uniform current collection, higher FF, and lower hot-spot risk at the module level.

Fig. 15

But mass-production hurdles remain:

  • LIF equipment investment: while replacing the sintering furnace, you add a laser + power supply + control system. Equipment vendor pricing decides the economics.

  • Line integration complexity: LIF must seamlessly dock with the plating line, and cycle-time matching (the paper uses a 20 m/s scan speed) needs validation.

  • GW-scale consistency: the paper is at lab/pilot level; yield stability at large-scale mass production still needs supporting data.

8. Comparison with Aiko ABC

Two paths, two stories

ItemAiko ABCTOPCon + LIF Copper Plating
Cell structureFull back-contactFront + rear
Laser grooving requiredNoYes
Laser damage issueNoneYes, but LIF can repair damage and optimize contact simultaneously
Metallization processCu/Ni/Sn platingNi/Cu plating + LIF
Mass-production statusAlready in mass productionLab / pilot

Aiko's BC architecture naturally avoids the laser-grooving pitfall. TOPCon cannot avoid it, but LIF offers a "fill-the-pit + optimize" combo solution — not only repairing damage, but also saving a process step and improving uniformity.

9. Summary

Where things stand

This new paper from Jiangnan University proves one thing: the laser damage in TOPCon copper plating can not only be repaired, but LIF repairs it better than traditional annealing — and along the way it also solves the uniformity problem of low-temperature sintering.

Efficiency gain of +0.45% abs., Voc gain of 0.86mV, and major improvement in contact resistance uniformity — these three numbers are worth a serious evaluation on any production line.

The mass-production threshold still exists, but the technical roadmap is becoming clearer.

Discussion topic: Is LIF replacing low-temperature sintering the "final kick" for mass-producing TOPCon copper plating, or just a "lab-side icing on the cake"?


Reference information:

TOPCon Copper Plating Takes Another Step Forward: LIF Replaces Sintering, Efficiency +0.45% abs., Voc Damage Repaired

  • Title: Integration of laser-induced firing with Ni/Cu plating for TOPCon solar cell metallization

  • Authors: Jingyun Zhang, Xi Xi, Jianbo Shao et al. (Jiangnan University + Jiangsu Xianghuan Technology + DR Laser)

  • Journal: Solar Energy Materials and Solar Cells

  • Year: 2026

  • DOI: 10.1016/j.solmat.2026.114198

Ooitech's View

Ooitech believes: LIF turns laser-damage repair and sintering uniformity into a single step, making TOPCon copper plating a meaningfully more viable route to silver-free mass production.

Further reading and background data

Public reference material on this topic, published by the organisations that maintain the industry's technology roadmap and market data:


Tags :

Request A Quote

All uploads are secure and confidential.

Type the characters shown in the image beside this field.
Verification code image, click to refresh
Why Choose Us

We deliver expertise you can trust our service

Direct-from-Factory Equipment.

Cost-Effective Advantages

We deliver exceptional value, maximizing results while optimizing budgets for clients.

Our Experience Team

Our skilled professionals specialize in innovative solutions and tailored strategies.

15+ Years Industry Experience

Deep expertise ensures reliable, trend-aware, and proven outcomes for success.

Testimonials

What Our Client Say's about us

Client testimonials praise our deep understanding of their challenges, which leads to innovative solutions and strong ROI. Long-term collaborations—some over a decade—demonstrate their trust and satisfaction. Their success stories drive us to continually exceed expectations. Know More

Our Products

Our Latest Products

Solar Tempered Glass: 93.5% Transmittance, Low-Iron
2025-09-08 14:17:29

Solar Tempered Glass: 93.5% Transmittance, Low-Iron

Solar tempered glass for PV modules: ultra-clear low-iron glass with anti-reflective coating, reaching 91.5%+ light transmittance in G1/M6/M10/M12 sizes.

Read More
C350-SZM Ribbon Busbar Bend Cutting Machine: 2-8mm
2025-09-08 14:46:07

C350-SZM Ribbon Busbar Bend Cutting Machine: 2-8mm

C350-SZM busbar bend cutting machine – programmable single/dual bending for tin-plated copper busbars. Supports double glass &

Read More
IEC 61215 & 61730 Test Equipment: 0.1-10kV, 2600mm
2025-09-08 14:12:26

IEC 61215 & 61730 Test Equipment: 0.1-10kV, 2600mm

Ooitech offers a complete range of solar panel testing equipment for IEC61215 and IEC61730 certification, including visual inspection stations

Read More
Solar Cell Laser Cutting Machine — OLS-20E Dual Laser
2025-08-17 17:41:21

Solar Cell Laser Cutting Machine — OLS-20E Dual Laser

Solar cell laser cutting machine for shingled cells: OLS-20E runs two laser heads with automatic 1/4 break, cutting kerf loss and micro-cracks on MBB.

Read More
Single Layer Double Chamber Automatic BIPV Laminator
2025-09-06 11:41:22

Single Layer Double Chamber Automatic BIPV Laminator

Ooitech OTCY-2754DD Single Layer Double Chamber Automatic BIPV Laminator features 2700x5400mm dual lamination areas, upper and lower double heating

Read More
BC Cell Tabber Stringer: 1000 Cells/h for IBC, ABC, HPBC
2025-08-17 17:41:21

BC Cell Tabber Stringer: 1000 Cells/h for IBC, ABC, HPBC

A BC cell tabber stringer welds IBC, ABC and HPBC cells on the rear face: 0.2 mm placement, 1000 cells/h, 0.2% breakage on Class A wafers.

Read More
AI research shortcut

Ask AI About OOITech

One click opens your AI assistant with a question about our solar panel production lines already filled in — the turnkey PV module lines we build, from semi-automatic to GW-scale, and what a quote needs.

Get a Quote