Solar Module Stringing: Cold Solder Troubleshooting

Editorial responsibility for this article rests with Wuhan Ooi Photoelectric Technology Co., Ltd. Written and reviewed by the Ooitech editorial team. See our editorial policy for how we write, where AI tools are used, and how to request a correction.

Solar Module Stringing: Cold Solder Troubleshooting

Quick answer: Stringing is the step where individual solar cells are soldered into a series string, and it sets both the module's power and the ceiling on line yield. A tabber places and solders ribbon onto each cell; a stringer then lays those cells in sequence and joins them. Because a cracked cell or a cold solder joint cannot be repaired downstream, everything that goes wrong here is written into the finished module. Practical stringing work comes down to four variables: cell format flexibility, busbar count for multi-busbar layouts, ribbon placement accuracy, and breakage rate. Ribbon thickness matters too — thinner ribbon lowers material cost and raises resistance, so there is a floor below which the efficiency gained at the cell is lost again at the joint. Machine platforms such as the ATW050 class handle multiple cell formats without a line change.

PV Module Manufacturing · by Jerry, Ooitech

Product Introduction

Solar Module Stringing: A Practical Guide to Troubleshooting Cold Solder Joints (With Mind Map)

No long intro. The mind map goes first. If it helps, save the article and download the image. You can also reach out through the WeChat backend to join the PV module tech chat group for the high-res version. (Just tell us which part you handle, like process, quality, equipment, or production.)

Before we get into cold solder troubleshooting, let's walk through how stringing actually works. The ribbon, pulled by the drawing mechanism, is placed precisely right above the busbar of the cell. Then the welding fixture comes down, and the press pins on the fixture apply pressure to the ribbon so it touches the busbar. The cell moves under the light box of the stringer, where infrared heats the ribbon and the cell. The tin on the ribbon melts and bonds with the silver paste on the busbar, forming a metal alloy.

One thing to keep in mind. For any cold solder inspection, check for exposed white (unbonded) areas first. If you see exposed white, deal with that before you judge the soldering itself. Everything below uses TOPCon cell stringing and the ATW050 stringer as the example.

Solar Module Stringing: A Practical Guide to Troubleshooting Cold Solder Joints (With Mind Map)

As shown, the first, second and third ribbons inside the red box are exposed white. The fourth one outside the box is normal.

Technical Parameters

1. Front full-panel cold solder

When the whole front side shows cold solder, check these:

ItemWhat to look at
Light boxFocus on the soldering parameters. Is the light box aging? Look at anything that affects the whole panel's heating.
Welding heightOn stop, the light box lifts a bit to avoid over-soldering the cell underneath. If the gap between the light box and the welding platform is too big during soldering, infrared efficiency drops and you get cold solder.
Time and powerSoldering time and light box power are the big factors. Check these first.
Flux concentrationAbnormal flux, especially too low, fails to clean the oxide off the ribbon surface, and soldering quality drops into a full-panel cold solder.
Incoming materialCells with too little silver paste cause cold or over solder. Uneven tin coating on the ribbon means the thin spots can't bond well with the paste. Expired or degraded flux won't remove oxides and the joint fails.
FixtureIs the fixture centered? An off-center fixture means the press pins can't hold the ribbon against the busbar, leaving a gap and cold solder. Also check the press pins themselves.

Solar Module Stringing: A Practical Guide to Troubleshooting Cold Solder Joints (With Mind Map)

16BB welding fixture

2. Front single-ribbon cold solder

Since it's a single ribbon, just check the mechanism tied to that specific ribbon.

ItemWhat to look at
DrawingLoose draw clamp, damaged clamp, or bad clamp bearing. Any fault on that single ribbon's mechanism puts the ribbon out of position and hurts the joint.
LiftingForeign matter in the lifting guide slot, or the ribbon scraping inside the slot.
FixtureFixture normal? Fixture pad worn? Press pin abnormal?
Light tubeFor cold solder at a fixed spot, check the light tube at that position for aging or wrong power.
CutterAfter cutting, does the ribbon have bends or burrs? Both make the ribbon scrape on the belt or other parts and ruin the joint.

Solar Module Stringing: A Practical Guide to Troubleshooting Cold Solder Joints (With Mind Map)

10BB stringer drawing mechanism

3. Front head cold solder

ItemWhat to look at
Light boxIs the shading plate deformed or blocking the light tube? Wrong shading plate position lets the ribbon melt tin before it enters the light box, that is premature tin melting, and you get head cold solder. Check the standby power and soldering time of the light tube.
FixtureIs the fixture arched or deformed? An arched fixture can't press the ribbon, so cold solder shows up. Do all press pins hold the solder head? Is the fixture slipping?
RibbonDeformed or over-stretched ribbon bends and can't line up with the busbar, causing cold solder. Also check for lifted ribbon ends, which can't touch the busbar.
OtherWas the moisture dried after cell cutting?

Solar Module Stringing: A Practical Guide to Troubleshooting Cold Solder Joints (With Mind Map)

Solar Module Stringing: A Practical Guide to Troubleshooting Cold Solder Joints (With Mind Map)

4. Head and tail spot cold solder

ItemWhat to look at
DrawingLifted ribbon end or over-stretched ribbon.
FixturePress pin fallen off, deformed, or stuck. Spot cold solder usually comes from a press pin problem. Without the pin, the ribbon can't reach the busbar.
FlatteningFlattening too close to the loading area, or flattening flipping over.

5. Back-side cold solder

ItemWhat to look at
AdsorptionWhen the base plate adsorption is off, the cell and ribbon shift relative to each other while moving, causing back cold solder. (Usually full back-side.)
Welding base platePoor base plate levelness or heavy wear. Is the base plate magnet lifted? Do the cell and base positions match?
Tail clampTail clamp too low, stuck, unable to grip the ribbon, or foreign matter inside.
LiftingLifting stuck, cylinder damaged or leaking, or abnormal ribbon sealing, so the ribbon bounces and shifts and doesn't seat right.
Welding beltWorn belt, lifted edges, or foreign matter under the belt shifts the back ribbon while the cell and fixture move. (Nothing else affects it. The front ribbon is held by the fixture and won't shift easily.)
OtherBad incoming cells or bad incoming ribbon.

Solar Module Stringing: A Practical Guide to Troubleshooting Cold Solder Joints (With Mind Map)

Guess how many BB this lifting jig is for. (PS: haven't used it in half a year.)

Technical Advantages

  • Logic-first troubleshooting: always check exposed white before judging the joint, so you fix the real defect not the symptom

  • Location-based method: front full-panel, single ribbon, head, tail spot and back side each have their own checklist, so you narrow down fast

  • Root-cause coverage: light box, drawing, lifting, fixture, ribbon, flux, base plate and belt are all mapped to specific defect types

  • Real-line reference: built around TOPCon cells and the ATW050 stringer, matching what operators actually see on the floor

Product Application

This troubleshooting logic applies across mainstream module lines. On the front side, the light box, fixture centering and flux concentration usually explain full-panel issues, while single-ribbon and head defects point back to the drawing and cutting mechanisms. On the back side, adsorption, base plate levelness and belt condition are the usual suspects. Whether you run a 10BB, 16BB or MBB stringer, the same defect-to-mechanism mapping keeps process, quality, equipment and production teams on the same page during a cold solder chase.

Ooitech's View

What we see on real lines matches this guide closely: most cold solder complaints trace back to fixture centering and flux state long before the light box itself is to blame, so checking exposed white first saves a lot of wasted teardown time. TOPCon busbars are thinner and the silver paste window is tight, which is exactly why ribbon flatness and press-pin condition matter more than they did in the PERC days. We tune these parameters during commissioning and operator training for every module line we deliver, and if you want to see stringing setups like the ATW-style flow in action, the Ooitech YouTube channel at www.youtube.com/ooitech has plenty of factory footage worth a look.

Note: the article references ATW's "Summary of Soldering Defects".

Further reading and background data

Public reference material on this topic, published by the organisations that maintain the industry's technology roadmap and market data:


Tags :

Request A Quote

All uploads are secure and confidential.

Type the characters shown in the image beside this field.
Verification code image, click to refresh
Why Choose Us

We deliver expertise you can trust our service

Direct-from-Factory Equipment.

Cost-Effective Advantages

We deliver exceptional value, maximizing results while optimizing budgets for clients.

Our Experience Team

Our skilled professionals specialize in innovative solutions and tailored strategies.

15+ Years Industry Experience

Deep expertise ensures reliable, trend-aware, and proven outcomes for success.

Testimonials

What Our Client Say's about us

Client testimonials praise our deep understanding of their challenges, which leads to innovative solutions and strong ROI. Long-term collaborations—some over a decade—demonstrate their trust and satisfaction. Their success stories drive us to continually exceed expectations. Know More

Our Products

Our Latest Products

DH200-Y Automatic Bussing Machine: 17s Cycle Time
2025-09-05 22:15:30

DH200-Y Automatic Bussing Machine: 17s Cycle Time

Ooitech DH200-Y Automatic Bussing Machine delivers high-speed electromagnetic busbar soldering with 17s cycle time

Read More
Full Automatic Solar Panel Production Line Equipment
2025-09-06 11:32:53

Full Automatic Solar Panel Production Line Equipment

Ooitech full automatic solar panel production line covers glass loading, EVA laying, string layout, tape sticking, lamination, trimming, framing

Read More
OTCY-2754DD BIPV Laminator: Double-Chamber, Single-Layer
2025-09-06 11:45:28

OTCY-2754DD BIPV Laminator: Double-Chamber, Single-Layer

Ooitech solar panel laminator full catalogue: 10 models, technical specs comparison, system descriptions, safety controls

Read More
Solar Panel Manufacturing Equipment: What to Buy First
2026-10-29 12:53:07

Solar Panel Manufacturing Equipment: What to Buy First

Solar panel manufacturing equipment buying guide: core stations vs auxiliary plant, what to buy later, budget phasing, spares, FAT/SAT, vendor checks.

Read More
Robot String Cell Layup HS-PBR: 5s/String, ±0.3mm
2025-09-05 22:01:28

Robot String Cell Layup HS-PBR: 5s/String, ±0.3mm

Ooitech HS-PBR Robot String Cell Layup Machine delivers high-precision automated string cell arrangement with ±0.3mm accuracy and ≤5s cycle time per

Read More
OPT-M960B EL & VI Tester: 0.1mm/pixel, Intel i7
2025-09-06 11:38:03

OPT-M960B EL & VI Tester: 0.1mm/pixel, Intel i7

Ooitech offers professional solar panel EL tester and VI tester machines (OPT-M960B, OPT-M951B, OPT-M950B) with SONY industrial cameras

Read More
AI research shortcut

Ask AI About OOITech

One click opens your AI assistant with a question about our solar panel production lines already filled in — the turnkey PV module lines we build, from semi-automatic to GW-scale, and what a quote needs.

Get a Quote