Why TOPCon Beat HJT: Path Dependence Explains

Editorial responsibility for this article rests with Wuhan Ooi Photoelectric Technology Co., Ltd. Written and reviewed by the Ooitech editorial team. See our editorial policy for how we write, where AI tools are used, and how to request a correction.

Why TOPCon Beat HJT: Path Dependence Explains

Quick answer: TOPCon beat HJT in the market for reasons that had less to do with cell physics than with path dependence. Both architectures raise efficiency above PERC, and HJT held an early efficiency advantage. TOPCon won because it could be added to an existing PERC line — boron diffusion, tunnel oxide and polysilicon deposition on top of equipment the manufacturer already owned — while HJT requires replacing the thermal process with a low-temperature sequence. The cost of that replacement was the deciding number: converting a line meant committing capital against a technology the rest of the supply chain had not yet standardised. Industry discussions at the time put the conversion decision in the hundreds of RMB millions range per line. The outcome illustrates that in manufacturing, compatibility with installed capacity usually outweighs a modest performance lead.

PV Module Manufacturing · by Jerry, Ooitech

Introduction

How to Choose the Right <a href=TOPCon Solar Panel Production Line Equipment -" title="Why TOPCon Beat HJT: Path Dependence Explains the Solar Cell Technology Race"/>

In 2023, many solar cell manufacturers faced the same boardroom question: if the industry must move from P-type PERC to N-type technology, should the next investment go to TOPCon or HJT?

On paper, HJT looked elegant. It had strong passivation, low-temperature processing, excellent bifacial performance, and a promising theoretical ceiling. But in real factories, the decision was often made by one number: the cost of conversion.

For a company already running PERC lines, upgrading to TOPCon could cost roughly RMB 50-80 million per GW. Building a new HJT line often required RMB 200-350 million per GW, even though equipment prices have been falling. That difference was too large to ignore.

So TOPCon did not win simply because it was the most advanced technology. It won because the road from PERC naturally led to TOPCon.

The core idea

The solar industry did not choose TOPCon in a vacuum. It chose TOPCon under the weight of ten years of PERC equipment, PERC engineers, PERC suppliers, PERC quality data, and PERC production habits. This is a textbook case of path dependence.

Technical Parameters

Market and technology comparison

ItemTOPConHJTBC
Main industrial positionDominant N-type routeHigh-potential challengerPremium and third-route contender
2025 estimated module output shareAbout 77.1% globallyMuch smaller shareSmaller but growing
2025 estimated cell shipmentAbout 320GWAbout 48GWAbout 36GW
Mass production efficiencyAround 25.5-26.5%Above 27% in leading linesDepends on route, strong premium potential
Typical PERC compatibilityHighLowMedium to low, depending on TBC or HBC design
Upgrade cost from PERCAbout RMB 50-80 million/GWUsually new line requiredHigher than TOPCon, complex process
New equipment investment pressureLower for existing PERC playersHighHigh to medium-high
Key process difficultyBoron diffusion, passivated contact, metallizationLow-temperature thin film, TCO, low-temperature pastePatterning, laser opening, masking, alignment
Main advantageFast industrial scale-upBetter structure for tandem potentialNo front grid, lower optical loss, premium appearance
Main weaknessEfficiency improvement is slowingWeak legacy compatibilityProcess complexity and yield challenge

Why the cost gap mattered

DimensionTOPConHJT
Switching costLow: partial PERC line upgradeVery high: largely new production line
Equipment continuityMany PERC tools and factory practices can be reusedEquipment system is substantially different
Talent basePERC engineers can adapt fasterRequires new thin-film and low-temperature process thinking
Supply chainQuickly inherited and expanded from PERC ecosystemNeeds separate paste, target, TCO, and process ecosystem
Yield ramp-upEasier for PERC-based manufacturersHigher learning cost and higher ramp-up risk

Technical Advantages

Path dependence: the hidden force behind TOPCon's victory

Path dependence means that today’s decision is heavily shaped by yesterday’s investment. Once an industry has built equipment, trained people, written standards, accumulated failure data, and optimized supply chains around one route, it becomes expensive and risky to jump to another.

TOPCon received all three layers of path dependence from PERC.

  • Lower switching cost: TOPCon only required several major new process modules on top of existing PERC lines, such as boron diffusion and LPCVD or PECVD passivated contact steps.

  • Positive feedback loop: More TOPCon lines encouraged equipment makers, paste suppliers, process engineers, and quality teams to improve TOPCon faster.

  • Lock-in effect: Once TOPCon became the mainstream language of production, talent, standards, troubleshooting, and supplier development all started flowing in the same direction.

TOPCon became stronger because more factories chose it. More factories chose it because it became stronger. That loop was decisive.

Why HJT lost the industrial race, not the technology race

HJT did not lose because it was a poor technology. In many ways, it is technically attractive.

  • Symmetrical structure supports strong bifacial performance.

  • Intrinsic amorphous silicon provides excellent passivation.

  • Low-temperature processing can reduce thermal stress.

  • Lower temperature coefficient helps performance in hot climates.

  • HJT has strong compatibility with future perovskite tandem cells.

But HJT had a serious industrial problem: it did not inherit the PERC production base.

A factory choosing HJT had to consider replacing large parts of existing assets, retraining engineers, building a new supplier system, accepting a new yield ramp-up cycle, and taking greater investment risk. In a period when solar manufacturing margins were under pressure, this was not just a technology decision. It was a survival decision.


BC: the third route, but not an easy shortcut

BC technology is often described as another possible winner, but its path is different from both TOPCon and HJT.

BC cannot fully inherit the traditional PERC structure because back-contact architecture changes the cell design fundamentally. It needs patterning, laser opening, masking, and precise back-side contact formation. That makes it much more complex than TOPCon.

However, BC can attach itself to different base technologies:

  • TBC: TOPCon plus back contact, sharing some TOPCon process and equipment logic.

  • HBC: HJT plus back contact, combining HJT passivation with back-contact structure.

BC is not simply a crossroads. It is more like a new highway that can carry different types of vehicles. But the highway itself still has to be built, and that is expensive.

The key problem is yield. Every extra process step can become a yield killer. Until BC can bring yield, cost, and throughput close to TOPCon levels, it will remain strong in premium markets but difficult to replace TOPCon at massive scale.

Product Applications

What this means for solar manufacturers

For manufacturers planning new cell or module capacity, the TOPCon-HJT-BC debate is not only about cell efficiency. It is about factory economics.

  • Existing PERC-based producers naturally moved toward TOPCon because the upgrade route was clearer.

  • New entrants with enough capital may consider HJT or BC, but they must accept higher process risk.

  • Premium module makers may use BC to target distributed generation, rooftop aesthetics, and high-efficiency segments.

  • Long-term technology investors are watching HJT-perovskite and TOPCon-perovskite tandem routes closely.

What this means for production engineers

For front-line engineers, the next three years are likely to remain TOPCon-heavy. The most valuable practical skills will still be related to full-process TOPCon control.

Important areas include:

  • Pre-cleaning and surface preparation

  • Boron diffusion control

  • BSG removal

  • LPCVD or PECVD passivated contact formation

  • Annealing process windows

  • Al₂O₃ and SiNₓ film deposition

  • Metallization and paste matching

  • Failure analysis and yield improvement

At the same time, engineers should not ignore perovskite tandem progress. The key indicators to watch are not only lab efficiency, but also stability, large-area performance, and process repeatability.

The perovskite tandem turning point

Path dependence is powerful, but it is not permanent. It can break when the performance gain of a new route becomes large enough to justify the switching cost.

This is why perovskite tandem matters. If tandem technology reaches stable industrial production, the old debate between single-junction TOPCon and single-junction HJT may become less important. The industry may shift from optimizing crystalline silicon alone to rebuilding the whole efficiency ceiling.

HJT supporters are betting heavily on this. HJT’s low-temperature process and symmetrical structure make it naturally suitable for perovskite tandem integration. But TOPCon companies are also developing tandem solutions, so HJT is not the only possible winner.


Contact and Purchase

Three clear judgments

First, TOPCon will remain the mainstream route in the next three years. From 2026 to 2029, TOPCon is likely to keep more than 70% market share. Its advantage is not only efficiency. It is equipment availability, trained engineers, supplier maturity, quality databases, and lower upgrade risk.

Second, HJT needs perovskite tandem to create a real comeback. If HJT remains only a single-junction technology, it will struggle to reverse TOPCon’s industrial scale. If perovskite-HJT tandem reaches stable mass production, the story may change.

Third, BC is TOPCon’s strongest structural threat if it solves yield and cost. BC has visible advantages in appearance and optical loss reduction, especially for high-end rooftop and distributed applications. But unless the process becomes stable and affordable, it will stay as a premium route rather than a universal replacement.

Final thought

The best technology does not always win first. The technology that fits the existing road often wins faster.

TOPCon beat HJT not because HJT lacked potential, but because PERC’s decade-long industrial accumulation pointed directly toward TOPCon. Equipment, engineers, suppliers, process windows, and factory habits all pushed in the same direction.

HJT now needs a large enough technology dividend to pull the industry away from its historical path. BC is trying to build its own path through heavy investment and process maturity. Perovskite tandem may become the next real turning point.

Ooitech's View

As an equipment-side observer, Ooitech sees TOPCon’s rise as a reminder that solar technology transitions are decided on the production floor, not only in efficiency charts. For module manufacturers, the winning route must match equipment continuity, yield ramp-up speed, material availability, and operator learning curves. The next disruption will likely come only when tandem technology offers a performance jump large enough to overcome today’s TOPCon lock-in.

Further reading and background data

Public reference material on this topic, published by the organisations that maintain the industry's technology roadmap and market data:


Tags :

Request A Quote

All uploads are secure and confidential.

Type the characters shown in the image beside this field.
Verification code image, click to refresh
Why Choose Us

We deliver expertise you can trust our service

Direct-from-Factory Equipment.

Cost-Effective Advantages

We deliver exceptional value, maximizing results while optimizing budgets for clients.

Our Experience Team

Our skilled professionals specialize in innovative solutions and tailored strategies.

15+ Years Industry Experience

Deep expertise ensures reliable, trend-aware, and proven outcomes for success.

Testimonials

What Our Client Say's about us

Client testimonials praise our deep understanding of their challenges, which leads to innovative solutions and strong ROI. Long-term collaborations—some over a decade—demonstrate their trust and satisfaction. Their success stories drive us to continually exceed expectations. Know More

Our Products

Our Latest Products

OTCT Solar Cell Tester: IEC 60904-9 A Grade
2025-09-08 13:53:04

OTCT Solar Cell Tester: IEC 60904-9 A Grade

OTCT-A solar cell tester – A-grade spectrum xenon lamp, 16-bit 4-ch acquisition, IEC60904-9:2020. Accurate IV curve measurement for mono &

Read More
Solar Cell Layup Machine WS-CL80D: 48s Cycle, ±0.1mm
2025-09-05 21:51:39

Solar Cell Layup Machine WS-CL80D: 48s Cycle, ±0.1mm

Ooitech WS-CL80D Automatic Solar Cell Layup Machine features dual gantry dual-gripper independent operation, linear motor driven main axis with 0.01mm

Read More
PV Ribbon Machine — Wire Drawing and Tinning Line
2026-05-11 16:34:01

PV Ribbon Machine — Wire Drawing and Tinning Line

The photovoltaic ribbon wire drawing and tinning integrated line: how round and flat solar ribbon is drawn, coated and wound in one pass, with checks.

Read More
OTCY-2754DD BIPV Laminator: Double-Chamber, Single-Layer
2025-09-06 11:45:28

OTCY-2754DD BIPV Laminator: Double-Chamber, Single-Layer

Ooitech solar panel laminator full catalogue: 10 models, technical specs comparison, system descriptions, safety controls

Read More
Automatic Layout & Bussing Integrated Machine
2026-03-24 17:53:42

Automatic Layout & Bussing Integrated Machine

Ooitech ALU-HBL Automatic Layout & Bussing Integrated Machine combines cell string positioning, layout, and electromagnetic busbar welding in one

Read More
Solar Cells for PV Modules
2025-09-09 09:29:14

Solar Cells for PV Modules

Solar cell processing equipment for PERC, TOPCon, HJT & BC cells – cutting, stringing, testing. Supports G1/M6/M10/M12 sizes.

Read More
AI research shortcut

Ask AI About OOITech

One click opens your AI assistant with a question about our solar panel production lines already filled in — the turnkey PV module lines we build, from semi-automatic to GW-scale, and what a quote needs.

Get a Quote